EN 1.4547Product form: Seamless Pipes (Sandvik Produced)

Sandvik 254SMO | UNS S31254

14 Product variants for grade EN 1.4547
Catalogue code Outside Diameter, inch Schedule Wall Thickness Stock
TST-254SMO-1/2-SCH40 1/2 40 In stock
TST-254SMO-3/4-SCH40 3/4 40 In stock
TST-254SMO-1-SCH10 1 10S In stock
TST-254SMO-1-SCH40 1 40 In stock
TST-254SMO-11/2-SCH10 11/2 10S Incoming stock
TST-254SMO-11/2-SCH40 11/2 40 In stock
TST-254SMO-2-SCH10 2 10S Incoming stock
TST-E-254SMO-2-SCH40 2 40 In stock
TST-254SMO-2-SCH80 2 80 Incoming stock
TST-254SMO-3-SCH10 3 10S In stock
TST-254SMO-3-SCH80 3 80 In stock
TST-254SMO-4-SCH10 4 10S Incoming stock
TST-E-254SMO-4-SCH80 4 80 In stock
TST-254SMO-6-SCH80 6 80 In stock